Processing technology of monocrystalline silicon wafer

Jul 03, 2023 Leave a message

Feeding → Melting → Necked Growth → Shoulder Growth → Isometric Growth → Tail Growth
(1) Feeding: Put the polysilicon raw material and impurities into the quartz crucible. The type of impurities depends on the N or P type of the resistance. The types of impurities are boron, phosphorus, antimony and arsenic.
(2) Melting: After adding polysilicon raw materials into the quartz crucible, the crystal growth furnace must be closed and evacuated, then filled with high-purity argon to maintain a certain pressure range, and then turn on the power of the graphite heater to heat to the melting temperature (1420°C), the polysilicon raw material is melted.
(3) Neck growth: when the temperature of the silicon melt is stable, slowly immerse the seed crystal into the silicon melt. Due to the thermal stress when the seed crystal is in contact with the silicon melt field, dislocations will be generated in the seed crystal, and these dislocations must be eliminated by necking growth. Necking growth is to quickly lift the seed crystal up, so that the diameter of the grown seed crystal is reduced to a certain size (4-6mm). Since the dislocation line forms an angle with the growth axis, as long as the necking is long enough, the dislocation can grow out of the crystal surface, producing a crystal with zero dislocations.
(4) Shoulder growth: After the thin neck is grown, the temperature and pulling speed must be lowered so that the diameter of the crystal gradually increases to the required size.
(5) Equal-diameter growth: After the thin neck and shoulders are grown, the diameter of the ingot can be maintained between plus or minus 2mm by continuously adjusting the pulling speed and temperature. The part with a fixed diameter is called isodiameter part. Monocrystalline silicon wafers are taken from equal diameter sections.
(6) Tail growth: After the equal-diameter part is grown, if the ingot is separated from the liquid surface immediately, the thermal stress will cause dislocations and slip lines in the ingot. Therefore, in order to avoid this problem, the diameter of the ingot must be gradually reduced until it becomes a sharp point and separates from the liquid surface. This process is called tail growth. The grown crystal ingot is lifted to the upper furnace chamber to cool for a period of time and then taken out to complete a growth cycle.